Calcium sulphate with half a molecule of water per molecule of the salt (hemi-hydrate) is called plaster of paris (plaster of paris).
Preparation
plaster of paris is prepared by heating gypsum (CaSO4.2H2O) at 120°C in rotary kilns, where it gets partially dehydrated.
The temperature should be kept below 140°C otherwise further dehydration will take place and the setting property of the plaster will be partially reduced.
Properties
It is a white powder. When mixed with water (1/3 of its mass), it evolves heat and quickly sets to a hard porous mass within 5 to 15 minutes. During setting, a slight expansion (about 1%) in volume occurs so that it fills the mould completely and takes a sharp impression. The process of setting occurs as follows:
The first step is called the setting stage, and the second, the hardening stage. The setting of plaster of Paris is catalyzed by sodium chloride, while it is reduced by borax, or alum.
Uses
- In surgery for setting broken or fractured bones
- For making casts for statues, in dentistry, for surgical instruments, and toys etc
- In making black board chalks, and statues
- In construction industry
11 comments:
Incredible points. Sound arguments. Keep up the great work.
--------------------------------------------------
Portugal Mortgage Broker
Very helpful. Thanks
Warning computer with the with finger on in the future please unsubscribe me from your system
Useful article.
Thank you for sharing how to make plaster of paris.
Thank you for sharing how to make plaster of paris.
informative and useful article on plaster of paris
Informative and useful article on plaster of paris
It was really helpful.
Post a Comment